A516 Grade 70

Status
Not open for further replies.

AUME99

Mechanical
Jul 9, 2007
2
Is there a suitable substitute for A516 Gr 70 steel to be used in low temperature (-44 F) applications? A516 Gr70 only comes in sheets, and I have some structural shapes (platforms and ladders) that need to perform under these low temps.
 
Replies continue below

Recommended for you

ASTM A 516 Grade 70 material is supplied in plate form, not necessarily sheet product form. So, I don't see a problem.

Regarding ladders, there are ASTM specifications for fabrication of ladders based on OSHA requirements.

Suggest you review
F840-83(2003) Standard Specification for Ladders, Fixed, Vertical



 