I have a question, that ASTM A516-70N (Curve D) is good without impact test for 1.25" thick @-30oC per ASME BPVC VIII UCS-66.
But per API-650, ASTM A516-70N belongs to group V and only good for 1.25" @ -11oC without impact test.
It seems API 650 is more strict than ASME BPVC VIII.
Did I have any misunderstanding or can anybody explain the philosophy why API650 seems more strict?
Thanks.