boffintech
Civil/Environmental
Am inspector on a project with spliced joist-girders.
Problem #1 = A number of joist-girders were assembled and erected prior to the inspector being notified and, yep, the bolt assemblies were incorrectly marked for pre-tensioning verification by turn-of-nut method and as a result the inspector is unable to verify bolt pre-tension. Specifically, the bolts were not marked prior to tightening; only the turned element, the nut, and the structural member were marked. Since the bolt was not marked it is not possible to know if it turned while tightening the assembly.
Problem #2 = During observation the next joist-girder assembly/erection it was discovered that during tightening of the bolts that as tightening progressed, you guessed it, previously tightened assemblies loosened.
So basically i can write a great daily report which states i know jack and sh%&.
Question: If an A490 assembly is loosened during tightening of addition bolts can the lessened bolt be re-tighten or must it be replaced? My understanding of the spec is that once a tightened A490 bolt is lessened it can not be re-used.
Also, any ideas on the other issues? EOR is coming to project but a heads-up what be appreciated.
Problem #1 = A number of joist-girders were assembled and erected prior to the inspector being notified and, yep, the bolt assemblies were incorrectly marked for pre-tensioning verification by turn-of-nut method and as a result the inspector is unable to verify bolt pre-tension. Specifically, the bolts were not marked prior to tightening; only the turned element, the nut, and the structural member were marked. Since the bolt was not marked it is not possible to know if it turned while tightening the assembly.
Problem #2 = During observation the next joist-girder assembly/erection it was discovered that during tightening of the bolts that as tightening progressed, you guessed it, previously tightened assemblies loosened.
So basically i can write a great daily report which states i know jack and sh%&.
Question: If an A490 assembly is loosened during tightening of addition bolts can the lessened bolt be re-tighten or must it be replaced? My understanding of the spec is that once a tightened A490 bolt is lessened it can not be re-used.
Also, any ideas on the other issues? EOR is coming to project but a heads-up what be appreciated.