a449

Materials
Mar 10, 2008
1
Could anyone pls let me know the comparable european (or british) standard for ASTM A449 steel?
 
Replies continue below

Recommended for you

ASTM A449 - Standard Specification for Quenched and Tempered Steel Bolts and Studs

Class 8.8 is approximately equivalent to ASTM A449 bolts