Im looking for information on an alloy called A444.0. i would be grateful for mechanical properties and corrosion resistance.

thanks in advance.
 
A444.0 is a binary Al-7%Si gravity die casting alloy. Typical properties are:
[tt]
Property F Temper T4 Temper
--------- -------- --------
UTS (MPa) 165 160
YS (MPa) 76 70
elongation (%) 13 21
Hardness (HB) 50
Corrosion 1 1
[/tt]
Corrosion ratings (1-5, 1 is best) based on salt spray performance.

 
thanks alot

can you tell me your source for this, as we are trying to source as U.S equivalent of a casting handbook that we use in the UK. THe UK one lists all alloyw, chemical composition, properties, pattern shrinkage, uses etc.

 
Thanks alot both Corypad and tvp, I went to the site yesterday, it is exactly what im lookin for.
 