Hi,
I'm new at this forum.
I just have a quick question that someone here might be able to help me.
I have a client that is requesting some A36 Mod plate to have a CE value between 0.3 min to 0.33 max and I'm having no luck finding. I wanted to ask if this plate is something that might be common or if I will have a difficult time finding. The majority of the plate I'm needing is 3/16" thk to 3/4" x 96" x 240". I have ran into a few but they have all been 1/4" x 120" x 240". If anyone can guide me or at least tell me this is nearly impossible, I would really appreciate any advise.

Thanks,
CadChick