metengr;
Regarding using SA36 for ASME I equipment, i noticed that in thread No. 154527, your reply was as the following:-
Question 2Quote:
Can it it be used as metal backing on welds for pressure parts?
in a Sec I Fired or unfired?
Reply; No. If you review PW-5.1 of Section I, Part UW, it states that materials used in welded construction shall conform to one of the material specifications in Section II with allowable stress values. Well, SA 36 does have allowable stress values but you must read further that Section I limits the use of SA-36 to bar stock and for use as stays - See Section II, Part D notes G15, G18.;
I think there is a conflict between your repy at the top of this thread and your reply in the other one. Could you please explain to me.
I will repeat my question again.
Can A36 use as membrane wall (Non-pressure part) which will be welded to the wall tube (Pressure Part) in the boiler, although it is not permitted to be using for ASME I in accordance with ASME II Section D. Please advice.
for your information, the metal temperature could be around 400°C.
Regards,
Shofa