Hi,
in order o correctly fill a furnace I need the real value of A357 alooy density when it is melt (2.7 Kg/dm3 is the value for the solid state).
There are some value or some diagram that can shows this phisical quantity?
Thanks,
Michele

PS: I need some info about :
- maximum acceptable value of H2 after degassing of A357 aluminum alloy (? cm3/100g);
- relationship between H2 microporosity and elongation failure on A357 alloy.
Someone can help me?

Thanks a lot
 
Replies continue below

Recommended for you

Hi Mixel

From a thermodynamical database computations here what you want:

a357qf2.jpg


bettwen 680 and 710 °C :
T°C density (Kg/M3)
680 2402
690 2399
700 2396
710 2393

best regards
 