Hi!

Instead of A350 LF2 What material I can use? for example AISI 310 stainless steel or 316?

Thanks a lot.
 
Replies continue below

Recommended for you

That's very little info.
I thonk 304L and 316(L) will do the job.
 
Thanks for your reply.

Lets forget about the stainless steel..Any other carbon steel for using in ammonia pipeline as being flange..A350 LF2 is not very easy to find and purchase for me so that I need anything else instead of it..
 
The MDMT will define the carbon steel flange material. What is the MDMT?

 