A325 Type 1 calls for medium carbon, Q&T steel, type 2 low carbon martensitic Q&T steel. For both, min yield 81 ksi, min. ultimate 105 ksi.
Because the spec. is limited to 1.5" max. diameter, there is some question about what strength the application really requires - i.e. in ASTM A449, which is also a medium carbon Q&T bolt, diameters from over 1.5" to 3" have a min. yield of 58 ksi, and a min. ultimate of 90 ksi. That's a big jump in yield strength...
SAE J429 is not going to get you there either - that spec. only covers up to 1.5" diameter also. Furthermore, your vendor should have added "Grade 5" to his recommendation, because without that, you could have gotten plain carbon steel bolts ("Grade 1") with 33 ksi yield strength. Also, SAE specs may or may not "meet code" for your application.
Two recommendations for you: come back with what tensile/yield strength your fastener needs, and what the governing standards (if any) for your application are, and people here can help you figure out a spec. to purchase to.
Second recommendation -- if you need to purchase bolts to specific standards, find a different vendor, because the one you quoted doesn't sound like much of an expert!
Sorry I can't help you out more than that