Does anyone know where I could find 2" diameter threaded rod that meets ASTM A320 Gr B8M Class 2? The big problem is the mechanical requirements listed in ASTM only go up to 1-1/2" diameter but the footnote says that it's not meant to limit the size to 1-1/2". Great help that is, since they don't list a strength requirement for 2" no one wants to touch it. My feeling is if a vendor could certify that it meets the requirement shown for over 1-1/4" to 1-1/2" then that would be fine.
Failing this, does anyone know if 2" that meets same spec except B8 (304 SS) instead of B8M (316 SS) is available? Still have the same problem with the mechanical properties but I'm thinking 304 may be easier to get.
Failing this, does anyone know if 2" that meets same spec except B8 (304 SS) instead of B8M (316 SS) is available? Still have the same problem with the mechanical properties but I'm thinking 304 may be easier to get.