A304 Stainless Steel

Status
Not open for further replies.

lutein

Structural
Joined
Apr 24, 2002
Messages
136
Location
US
hi,
Does anybody know what is the material properties for A304 Stainless Steel - The Modulus of Elasticity, Yield and Shear Strength? How does it compared to 846M1 and 846M2 ?

PLease help....
Thank you in advance
 
AISI 304
YIELD STRENGTH 2% OFFSET 38,000 psi
ULTIMATE STRENGTH 90,000 psi
MOD. of ELASTICITY 28.0 X 10e6
 
Thank you very much
 