Anyone out there with A300-600 floor/ floor panel experience (e.g. how load makes it to SOB from seat tracks)?
 
What exactly are you looking for? We generally make our own panels because they are always messed up. Have you looked at the IPC, SRM or AMM to see how they are actually installed?
 