Hi,
I'm having a problem and I'm hoping someone on the board can give me a hand.
I've got a client with a design which has a flanged item constructed of A182 904L for a B31.3 component. I've looked through the allowables from App A and not found it and also Section II Part D with no luck. After some research online I've found that it has a UNS of N08904. This still isn't in B31.3 but I can find it Section II, Part D. There is also a listing in B16.5 for B649 N08904. I'm not sure how any of this relates as B649 is listed in B16.5 as a forging but as barstock in Section II Part D.
I was wondering if anyone had used this material before and where they went for allowable stresses and flange pressure ratings. I'm getting a little confused.
Thanks.
I'm having a problem and I'm hoping someone on the board can give me a hand.
I've got a client with a design which has a flanged item constructed of A182 904L for a B31.3 component. I've looked through the allowables from App A and not found it and also Section II Part D with no luck. After some research online I've found that it has a UNS of N08904. This still isn't in B31.3 but I can find it Section II, Part D. There is also a listing in B16.5 for B649 N08904. I'm not sure how any of this relates as B649 is listed in B16.5 as a forging but as barstock in Section II Part D.
I was wondering if anyone had used this material before and where they went for allowable stresses and flange pressure ratings. I'm getting a little confused.
Thanks.