The following are reported and estimated minimum mechanical properties for ASTM A 106 Grade B material at ambient temperature;
UTS - 60 Ksi
YS (0.2% offset) - 35 Ksi
Estimated Value
Shear yield point (0.58*35 Ksi) = ~ 20 Ksi
Ultimate Shear strength (0.75*60 Ksi) = ~ 45 Ksi
Bearing stress is not as mechanical property, it is a calculated value based on projected area * strength