Feb 10, 2025 #1 B Brooke William Industrial Joined Nov 7, 2024 Messages 6 I want to manufacture turbine blades with Waspaloy. What are the yield strength and tensile strength at 650°C, and do you have any recommendations?
I want to manufacture turbine blades with Waspaloy. What are the yield strength and tensile strength at 650°C, and do you have any recommendations?
Feb 10, 2025 #2 Gr8blu Electrical Joined Aug 18, 2021 Messages 803 Location US I take it you've already researched the "basic" properties of the material. https://www.specialmetals.com/documents/technical-bulletins/waspoloy.pdf Maybe graph the known data and see where the curve falls at the desired temperature condition? Upvote 0 Downvote
I take it you've already researched the "basic" properties of the material. https://www.specialmetals.com/documents/technical-bulletins/waspoloy.pdf Maybe graph the known data and see where the curve falls at the desired temperature condition?
Feb 10, 2025 #3 EdStainless Materials Joined May 20, 2004 Messages 16,395 Location Waukesha WI USA There is likely data for this alloy in MMPDS also. It has been around since the 50's so there is lots of data out there. Upvote 0 Downvote
There is likely data for this alloy in MMPDS also. It has been around since the 50's so there is lots of data out there.