Dear all
I am interested to know if i can convert a tubeless wheel rim to a tubed rim for a special equipment like road sweeper.
Will there be any difference in rim thickness apart from the visual difference of valve hole.
This will be a short term arrangement till I get the correct rim.
Regards
 
Replies continue below

Recommended for you

Given that people routinely fit inner tubes as a repair to tubeless tires, I'd say in practical terms you should be OK.

Cheers

Greg Locock


New here? Try reading these, they might help FAQ731-376
 
Of course, make sure the surface is smooth on the rim. You can get rim tape pretty cheap which is for this exact purpose.
 
Thanks hydroman247. What is the material of rim tape. Can that be sourced from tire dealer?
 
A tubeless rim will have a drop center so the tire can be buttonhooked on. The tubetype rim doesn't have this. My fear would be that the tube would want to inflate into that well.

However, the tube can be punctured by projections inside the rim. Sometimes they use a flap to prevent this - a thick slap of rubber put in after the tube inserted.

On the balance, I wouldn't recommend doing this on a log term basis, but I think it will work as a temporary solution.

And to answer the exact question you asked, the way tubetype tires and tubeless tires carry the load is exactly the same, so the rim thickness is immaterial.
 
Hi Bljnv,

Rim thickness is dependent on the wheel loads, and there isn't any difference between tubeless and tube tire loading. You haven't told us if you're using "J" configuration car/lt. truck rims or "K" medium truck rims, but the retention of the tire beads depends on inflation supplied tension stretching the beads into the seats. I'd chalk mark the tire position to the rim to make sure there's no slippage that would damage the tubes, and possibly increase the inflation pressure.

That said, the tube increase the rate of rapid air loss on blowouts and may pose a risk on some applications. If speeds are low, and vehicle control is not a concern, you should be OK
 