wich is the temperature range of the A 516 Gr.60 steel?
Can I use it for -10°C=>70°C air-pressure vassels (10bar/diameter 10inch)?
We would like to PED-certify our item. I know that I have to ask to my supplier:
- EN 10204 3.1.b certify
- a Quality System
- WPS for weldings

The question: do I have to ask my supplier for additional requirements such as:
1) Iso V Notch Impact test at -10 °C
2) High temperature (70°C) tensile tests??

Thanks
Carlo - Italy
 
According to the PED materals are considered ductile if they are capable of meeting 27 J at 20 deg. C
According to ASTM A 20 the material A 516 Gr. 60 can easaly fullfil this requirement. Actual impact testing would not be required.
Hot tensile testing is not required.
 
Thank you ijzer!
"According to ASTM A 20" ... you can suppose my next question ... can I find on the web the ASTM A 20 (or a part of it, to make evidence about your considerations).
carlo

cmontagnani@aeautel.it
 
ASTM A 20 is available from ASTM International at:


Regards,

Cory

Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
The requirement of Impact test on the Plate is based on the MDMT and the thickness of the vessel you are designing. Assuming the MDMT being -10 degree C, for the diameter you have specified, thickness is expected to less such that Impact test may not be necessary. Have a look at UCS 66 and UG 84 of ASME sec VIII Div 1.

Similarly tensile test at 70 degree is not necessary. Refer to ASME sec II D + UCS 23 table, the allowable stress of the material you have specified does not vary, and 70 degree centigrade is not considered high temp.