carloitaly
Electrical
- Oct 31, 2003
- 3
Hi,
wich is the temperature range of the A 516 Gr.60 steel?
Can I use it for -10°C=>70°C air-pressure vassels (10bar/diameter 10inch)?
We would like to PED-certify our item. I know that I have to ask to my supplier:
- EN 10204 3.1.b certify
- a Quality System
- WPS for weldings
The question: do I have to ask my supplier for additional requirements such as:
1) Iso V Notch Impact test at -10 °C
2) High temperature (70°C) tensile tests??
Thanks
Carlo - Italy
wich is the temperature range of the A 516 Gr.60 steel?
Can I use it for -10°C=>70°C air-pressure vassels (10bar/diameter 10inch)?
We would like to PED-certify our item. I know that I have to ask to my supplier:
- EN 10204 3.1.b certify
- a Quality System
- WPS for weldings
The question: do I have to ask my supplier for additional requirements such as:
1) Iso V Notch Impact test at -10 °C
2) High temperature (70°C) tensile tests??
Thanks
Carlo - Italy