Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

A 350 LF 6 Class 2

Status
Not open for further replies.

corvax

Petroleum
Oct 7, 2010
9
What means class 2 in this indication A 350 LF 6 class 2 - class of pressure ?
 
Replies continue below

Recommended for you

The class refers to the maximum allowable temperature.

-TJ Orlowski
 
Some clarification - the Class of material in this specification refers to specified minimum mechanical properties (strenght, ductility) and minimum impact energy value at 0 deg F.
 
Where can I find explenation in ASME
 
Correction - minimum impact energy at -60 deg F for LF6.
 
what value of impact of energy ?
 
Minimum of 15 ft-lbs for only one specimen of a set of three
or average of three specimens - minimum 20 ft-lbs.
 
corvax;
Read the specification! I just answered your question above.
 