Dear all,

I would like to know what the UNS Steel N° for A 194 Gr. 2H steel (if any) ? Perhaps I'm not luky or I'm blind but I've found it in ASME.

Thanks for help.
 
Replies continue below

Recommended for you

There may be some UNS number used under certain conditions, but I've never seen one and don't know how they could due to the allowed use of different metals to meet the physical specifications.

At the present manufactures are scrambling to get anything to make the nuts. Alloy bar is in short supply the world over.
 