Jun 27, 2020 #1 azadfar Industrial Joined Jan 15, 2015 Messages 7 Location IR Hello everyone, what electrode do you recommend for manual welding of 900A material with manual welding process?
Hello everyone, what electrode do you recommend for manual welding of 900A material with manual welding process?
Jun 27, 2020 #2 TugboatEng Marine/Ocean Joined Nov 1, 2015 Messages 12,064 Location US Crane booms are typically constructed from ASTM A514 steel with a 110ksi tensile strength. You can look up general procedures for that material but if it's on the crane boom you should only be using manufacturer approved procedures. Upvote 0 Downvote
Crane booms are typically constructed from ASTM A514 steel with a 110ksi tensile strength. You can look up general procedures for that material but if it's on the crane boom you should only be using manufacturer approved procedures.