Hello everyone, what electrode do you recommend for manual welding of 900A material with manual welding process?
 
Crane booms are typically constructed from ASTM A514 steel with a 110ksi tensile strength. You can look up general procedures for that material but if it's on the crane boom you should only be using manufacturer approved procedures.
 