Hello everyone, what electrode do you recommend for manual welding of 900A material with manual welding process?
 
Replies continue below

Recommended for you

Crane booms are typically constructed from ASTM A514 steel with a 110ksi tensile strength. You can look up general procedures for that material but if it's on the crane boom you should only be using manufacturer approved procedures.
 