Team Members "help asap"
We would like to request your advisor as below situlation;
We received the large fitting as 80" Elbow. But we didn't find any code to judge this fitting shape and dimesion like acceptance criteria during the receiving inspection.
So, Could you give us any information about this?
We checked the ANSI B16.9, & MSS-79. But there are only described to 48" size.
Would this fall under AWWA?
Leonard Thill, Pusan Korea