Apr 6, 2009 #1 abbver98 Mechanical Joined Jun 21, 2002 Messages 195 Location BE Bolt 8.8 and 12.9 mechanical properties at high temperature - what is the standard reference ? thanks
Bolt 8.8 and 12.9 mechanical properties at high temperature - what is the standard reference ? thanks
Apr 6, 2009 #2 gr2vessels Mechanical Joined Sep 29, 2004 Messages 1,971 Location AU Check this out (and thousands more on google) http://euler9.tripod.com/bolt-database/22.htmlCheers, gr2vessels Upvote 0 Downvote
Check this out (and thousands more on google) http://euler9.tripod.com/bolt-database/22.htmlCheers, gr2vessels
Apr 7, 2009 #3 SnTMan Mechanical Joined Jan 22, 2005 Messages 6,862 Location US abbver98, see ASTM F586M, which references other ASME / ASTM standards. Then see ASME Sec II, Part D for the stresses at temperature for the material of interest. Regards, Mike Upvote 0 Downvote
abbver98, see ASTM F586M, which references other ASME / ASTM standards. Then see ASME Sec II, Part D for the stresses at temperature for the material of interest. Regards, Mike
Jul 14, 2009 #4 chaboche Mechanical Joined Jun 11, 2007 Messages 35 Location GB Should that be ATM A568M? Upvote 0 Downvote