I am investigating manufacturing wheel spindles for a 320kg FSAE car out of 7xxx aluminium due to its good fatigue and strength properties. This part will be subject to cyclical bending and torsion although it will only experience limited track time since it will only be used for two years with 6 track days per year before it is decommisioned (approx 100,000 cycles).
Our FSAE team is based in Sydney, Australia and only 7075-T651 is readily available in 7xxx round bar. Will stress corrosion cracking be a significant issue for this kind of application? Is it possible to and should I get the spindles treated to a T73 temper after machining of the T651 round?