Hi all,
I'm currently researching a suitable material for a component I'm designing.
I've pretty much settled on 7075 aluminium, but I'm now seemingly faced with the choice between T6 or T73/T76. From what I can see, the T73/76 offers better resistance to SCC than the T6, but at a price of a reduction of around 10% in the proof and UTS.
Is this about right...or are there other things to consider between the two? I'm not a materials scientist by any manner of means, but I'm curious as to why the T7x temper seems to lose around 10% of its max Proof and UTS?
Any thoughts on any of the above would be very gratefully received.
Thanks
FP
I'm currently researching a suitable material for a component I'm designing.
I've pretty much settled on 7075 aluminium, but I'm now seemingly faced with the choice between T6 or T73/T76. From what I can see, the T73/76 offers better resistance to SCC than the T6, but at a price of a reduction of around 10% in the proof and UTS.
Is this about right...or are there other things to consider between the two? I'm not a materials scientist by any manner of means, but I'm curious as to why the T7x temper seems to lose around 10% of its max Proof and UTS?
Any thoughts on any of the above would be very gratefully received.
Thanks
FP