hello all,

I would like to ask the suitability of using 70/30 Cu-Ni piping in the sour environment and in the applications below.

thank you.




COOLING WATER, OPEN DRAINS (OILY),
CHEMICAL DRAINS, TREATED SEA WATER,
UTILITY WATER, OILY WATER,
BRACKISH WATER , WASH WATER,
FIRE WATER (BRACKISH)-BELOW GROUND DUTIES ONLY PRODUCED WATER
FIRE FIGHTING FOAM - BELOW GROUND DUTIES ONLY PROCESS CONDENSATE
BRINE WATER, EFFLUENT WATER,
DEDICATED DRAINS, WASTE WATER,
OILY BRINE,
 
All I have ever seen used for these applications is 90/10 Cu-Ni. Is this for offshore use?
 
this is for off shore use.

I scanned the link you provided, it helped me lot thanks.
I also need the wall thickness values for 1/2, 3/4, 1, 1 1/2 and 2 inch pipes for these applications.
 
You're asking WAY too much of a free forum.

If you need to calculate wall thicknesses and do not know how, then I very strongly suggest that you find an engineer experienced in this field, hire them, and pay them appropriate engineering fees.
 
shmulik thank you for your response.

I got what I want
 
Reference the EEMUA standards for Cu/Ni.
 