Looking at a new UT Thickness meter. I see some advertised as having the capability to go thru the paint. We have mostly done our inspections by wire wheel buffing the paint off down to bare metal and taking our readings from there. The ability to not have to buff off the paint (and re-apply paint after we are through) to take the readings would be a time and money saver.
What do you guys do?
What do you guys do?