Brokenwindow
Mechanical
I'm currently investigating root cause for problem with material cracking. It's Ø .622-1018 material with a ksi of 85000-105000. The cracks are happening in the inside (compression) of the bend. The wire is ran through a cnc bender and is bent around a .625 roller. We are seeing about a 3-6% crack rate.
KSI/machine speed/roller pressure/etc doesn't seem to be a factor.
We have ran DOE's through our bender and are currently looking at our material suppler for assistance. All material is with astm a510 standards.
Basically I'm looking for ideas/directions to investigate.
Thanks in advance..
KSI/machine speed/roller pressure/etc doesn't seem to be a factor.
We have ran DOE's through our bender and are currently looking at our material suppler for assistance. All material is with astm a510 standards.
Basically I'm looking for ideas/directions to investigate.
Thanks in advance..