Im looking at a job for a pool house and the eupitiment inside is mande with 6063 alum tubing. I wonderering if there is going to be a corrision issue with the chlorine?
 
Replies continue below

Recommended for you

Yes, you would get the following:

2 Al + 3 Cl2 = 2 AlCl3

Suggest having the aluminum chromated and powder coated.
 