We are having problems with welds cracking. We are welding 6061 T651 1/2" thick with 1/16th" 5556 filler using the GMAW process anyone have any input on why and possible prevention we are keeping the temp below the 250 degrees f. The weld sizes range from 1/4" to 3/8" fillets. We are tring to weld the 3/8" weld in one pass any suggestion would be great.