What is the recommended amount of hot dip galvanzing. Is 600 grams per m2 is acceptable, too less, or over kill
 
Replies continue below

Recommended for you

275 g/m2 is common hot dipped galvanizing. 600 is heavy and used for particularly corrosive environments. In Canada, these are referred to as Z275 and Z600 respectively.
 