Does anyone see any harm being done having PWHT performed on 6" sch 80 2.25cr (.432 thk P5a) piping even though it is not required by code?

Shop environment.
 
Replies continue below

Recommended for you

^ No extra expense (on our part anyways). Subcontractor made an in-house error.
 
One assumes the contractor has a WPS qualified with PWHT on P-5A material.
 