Could anyone provide me with basic properties such as tensile strength etc for 50MnT steel which is the material used for a gear I am about to use?
 
Are you sure that the steel's designation is not 50Mn7?
50Mn7 is a standard German steel somewhat like AISI1552 but with manganese in the range 1.60-2.00%.
 