Tank for fresh water storage. 1/4" welded plate. The tank is 20'x20'x12'. I was to use the H32 but not available right now so it was suggested I use H116. Whats the difference? Is the H116 suitable?

Thank-you
 
Replies continue below

Recommended for you

First time I'd heard of that temper. Matweb ( shows them being equivalent based on Aluminum Association data sheets, but I have no spec's. to back that up with.
 