I have an existing building with 48LA18 joists at 8'-0" spanning 88'-0". Does anyone have load capacity tables for this joist? circa 1963.
 
Replies continue below

Recommended for you

My copy of the 75 year Steel Joist Manual shows:
Max end reaction: 23,735 lbs
max load: 518 plf
Weighs: 61 plf