I've been looking for a stress strain curve for 440C stainless steel AMS 5630, and heat treated to AMS 2759/5 (55-60 Rc)and have been having no luck, does anyone know where to find one?

thanks
 
It will be a straight line from start to UTS, the slope will be about 30,000,000 psi.
This material has no significant yielding prior to failure.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
 