Dear all,
4340 steel
I’m having difficulties achieving hardness properties from a hot press forged section.
Forging from 1100C (2012F) with a greater the 4:1 reduction.
Following forging I’m annealing at 650C (1202) for 13hrs and furnace cooling at 50C per hour.
I need to achieve a hardness of no greater than 229HB but unfortunately its coming out up to 269HB.
Any ideas?
Thanks
4340 steel
I’m having difficulties achieving hardness properties from a hot press forged section.
Forging from 1100C (2012F) with a greater the 4:1 reduction.
Following forging I’m annealing at 650C (1202) for 13hrs and furnace cooling at 50C per hour.
I need to achieve a hardness of no greater than 229HB but unfortunately its coming out up to 269HB.
Any ideas?
Thanks