I have an application for a tool where the corrosion resistance of D2 steel is proving a problem.
A hardenable stainless such as 420 should be hard enough and at least let us avoid plating. The environment is industrial, humid and mildly corrosive (China).
A supplier put me on to the crucible 420MQ which is C0.38 Mn0.46 Si0.4 Cr13.6 V0.3 as a good corrosion resistant option.
Only problem is the supplier is in Europe so I need a European steel reference.
I think a 420 would equivalent be fine, does anyone know of a German equivalent?
A hardenable stainless such as 420 should be hard enough and at least let us avoid plating. The environment is industrial, humid and mildly corrosive (China).
A supplier put me on to the crucible 420MQ which is C0.38 Mn0.46 Si0.4 Cr13.6 V0.3 as a good corrosion resistant option.
Only problem is the supplier is in Europe so I need a European steel reference.
I think a 420 would equivalent be fine, does anyone know of a German equivalent?