16 pieces , 3" thick x 2" dia ( solid - big dounut); quenched in oil (1500F FOR 3 HOURS) ; TEMPERED AT 660 F for 2 1/2 hrs. Quenched vertically to minimize steaming that encapsulates the surface upon cooling ( 2" spacing between each piece). Furnace has controlled atmosphere , oil tank has agitation and cooling system , one test piece was made prior to production and the result was satisfactory. After quenching 16 at above conditions the hardness at surface was 43 Rc.Heat treatr claims that such an alloy cannot achieve 55Rc by quenching 16 at a time. Suggested increase austenitizing temperature to 1600 F. hE CLAIMSthe risk of cracking is high. What do you suggest should be done ?
ibf (mining)
16 pieces , 3" thick x 2" dia ( solid - big dounut); quenched in oil (1500F FOR 3 HOURS) ; TEMPERED AT 660 F for 2 1/2 hrs. Quenched vertically to minimize steaming that encapsulates the surface upon cooling ( 2" spacing between each piece). Furnace has controlled atmosphere , oil tank has agitation and cooling system , one test piece was made prior to production and the result was satisfactory. After quenching 16 at above conditions the hardness at surface was 43 Rc.Heat treatr claims that such an alloy cannot achieve 55Rc by quenching 16 at a time. Suggested increase austenitizing temperature to 1600 F. hE CLAIMSthe risk of cracking is high. What do you suggest should be done ?
ibf (mining)