Hi,
does anyone know if there is data available for a hardness vs temperature curve for 4140 steel at a certain time. I have been looking everywhere and cant seem to find it.

Your help would be much appreciated.

thank you

Paras
 
Replies continue below

Recommended for you

The ASM Heat Treater's Guide has a hardness vs. tempering temperature chart but my version does not show any time reference. What time are you looking for?
 
Anywhere between 2 and 72 hours will work. Another thing I forgot to mention was that is the 4140 material air cooled instead of quenched
 
Here you go.

it is on page 148


As for the time: 2 hours at temperature.

As for cooling from tempering temperture:
Air cooled is best. However, if it is not complex geometry or very thin it can be quenched. This won't affect the microstructure but will induce some residual stresses.

Design for RELIABILITY, manufacturability, and maintainability
 