gowrishankarz
Mechanical
Hello everybody,
We are having a lot of problems with heat treating round 4140 material. This part is .5" in dia & 25" long. It has a V groove machined into it. We just need the edges of the V groove to be hardened to about 55 Rc. Right now we are flam hardening the edges & this makes the part to bow severely. We then straighten the part in a manual press. I was wondering if it will be better to through harden the hole part instead of flame hardening? Is there any better way to straighten the part after heat treating? Can sombody help me with this?
Thank you
We are having a lot of problems with heat treating round 4140 material. This part is .5" in dia & 25" long. It has a V groove machined into it. We just need the edges of the V groove to be hardened to about 55 Rc. Right now we are flam hardening the edges & this makes the part to bow severely. We then straighten the part in a manual press. I was wondering if it will be better to through harden the hole part instead of flame hardening? Is there any better way to straighten the part after heat treating? Can sombody help me with this?
Thank you