Have been using a 5/16" hex 4140 steel bar for 2 yrs and now can't locate. The bar is used as an input shaft and must be heat treated to Rc 20-26 and straightened within .020 in a 15" length.
Does anyone know where I can find this material?
An alternate of 12L14, heat treated to same hardness has been proposed. Would this be an equivalent substitute? Do not have any experience with HT 12L14. Would it be more or less likely to warp?