I have an urgent request for choke line material, for export to Brazil.

Please advise who may be able to supply this item:

Need 3,300 feet of: 4" (1/2"or 5/8") wall ,4130 X-80. Lengths have to be in 10 meter sections or something that only has one weld in 65`length. This is for 10,000 maximum well pressure (MWP) and 15,000 psi test pressure.

Robert Young
(Santa cruz, Bolivia)