What are the chances of hot rolled plate, type 410 SS meeting impacts 35/40 @ -20F if first performing a Q & T treatment. No special chemistry controls were specified and just by memory I think the P was at .026. S .015.
If a heat treatment would likely work what would you suggest for a tempering temp. PWHT will be at 1400F for 1 hour.
Thanks,
If a heat treatment would likely work what would you suggest for a tempering temp. PWHT will be at 1400F for 1 hour.
Thanks,