Hi All,

What is the most commonly used standard for corrosion resistance testing of stainless type 410 S?
We are performing welding and heat treatments and would like to ensure corrosion resistance is not hampered.
 
Refer to ASTM G157, Outokumpu MTI-1 procedure;- use the documents referenced in these standards for further info.
Cheers,
gr2vessels
 
Cloa,

We are suplying 410S clad plates for coke drums application in refineries.
 
Thanks gr2vessels for this interesting reference.
 