Gentlemen:
I am to build a small water boiler
(1,000,000BTU/Hr); Temp: 250d.F.
The fuel is:
Wastewater digester gas (bio gas) 75% CH4 gas
-H2S content: 40 ppm (0.004%) of Sulfur as H2S form.
I am to choose the best carbon steel for the job or if not c/s will be stainless.
What about the burner materials? (a power burner will be used)
How rusty is this 40ppm (.004%)amount of sulfure?
Thanks, genb
I am to build a small water boiler
(1,000,000BTU/Hr); Temp: 250d.F.
The fuel is:
Wastewater digester gas (bio gas) 75% CH4 gas
-H2S content: 40 ppm (0.004%) of Sulfur as H2S form.
I am to choose the best carbon steel for the job or if not c/s will be stainless.
What about the burner materials? (a power burner will be used)
How rusty is this 40ppm (.004%)amount of sulfure?
Thanks, genb