Need some help, what is the minimum cover distance for a 4" concrete slab with #4 rebar. Trying to utilize slab for uplift
 
I'm not big on concrete, but, I've always used 3/4" or maybe more for fire resistance rating.

-----*****-----
So strange to see the singularity approaching while the entire planet is rapidly turning into a hellscape. -John Coates

-Dik
 